Details
AWS A5.18 ER70S-6
EN SG2 / SG3
GB/T 8110-2008 ER50-6
JIS Z3312 YGW12
Strong resistance to surface scales and oil stains on the base metal. It has low blowhole sensitivity.
Chemical Composition of Welding Wire(%)
C | Si | Mn | P | S | Cr | Ni | Cu | Mo | V | |
Sample Value | 0.07 | 0.91 | 1.52 | 0.013 | 0.014 | 0.017 | 0.110 | 0.011 | 0.003 | 0.003 |
Mechanical Properties of Deposited Matal
Yield Strength ReL(Mpa) |
Tensile Strength Rm(Mpa) |
ElongationA(%) |
Impact Test KV2 J |
||||
Standard | ≥420 | ≥500 | ≥22 | ≥27(-40℃) | |||
Sample Value | 459 | 548 | 29 | -30℃ | 90 | 87 | 93 |
Welding Positions